Ensuring proper care of concrete

After pouring the mortar and shaping the structure, it is very important to achieve the quality of concrete required by SNiP. The measures that ensure these parameters are determined to a greater extent by the cement assortment, air temperature and humidity (this depends on the weather), and to a lesser extent by the configuration of the product itself. For example, Portland cement concretes are moistened for seven days; for concretes based on other types of cement, the period of planned maintenance varies from two to fourteen days. On hot days, concrete maintenance takes longer than in cold weather. With proper care in the first days after pouring it, the required quality of the structure will be practically ensured. Temperature surges, shocks, loads, impacts, drying, instead of maintaining the required moisture level, will cause shrinkage deformations and, as a result, surface cracking, reducing the strength of concrete.

The peculiarity of the process of hardening of concrete mortar is that water penetrates into the volume of concrete mass containing cement particles gradually, and therefore the deposition of crystals formed during the hydration reaction takes quite a long time. That’s why concrete takes a long time to harden. The most optimal air parameters for natural hardening of concrete are temperatures from 18 to 22 degrees C with a relative humidity of at least 90%.

As already indicated, during rapid dewatering there is an increase in concrete shrinkage, leading to its cracking. To avoid this, the concrete must be constantly wetted. It is recommended to immediately cover the wet surface of the newly poured mortar with some moisture-retaining material such as matting or sawdust and not delay maintaining the required humidity, that is, begin to wet it after ten to twelve hours, and on warm days, 2-3 hours after the completion of pouring the concrete. It is strictly forbidden to direct powerful jets of water at recently laid concrete that has not yet properly set, so as not to wash it away; spraying through a sprayer is quite enough. To obtain the required moisture content, concrete must be wetted every one and a half to two hours in hot and windy weather, in cloudy weather - after three hours and at least two to three times a night. But at temperatures from zero to +5 degrees C, humidification is not allowed.

Moisture from concrete structures is lost not only from the open upper surface, but also from the lower supporting surface of the product in contact with the bulk base, so in this case the amount of moistening (watering) should be increased. To protect such areas, it is better to use polymer films.

In order not to provoke the formation of cracks and gouges on the drying corner edges of concrete structures and on the side surfaces from which the formwork has been removed, the same, only more carefully performed, regulated procedure is necessary - abundant moisturizing, if necessary, even using wet wiping.